Nanoindentation Assessment of the Interphase in Carbon Nanotube-Based Hierarchical Composites
Ana M. Díez-Pascual, Marián A. Gómez-Fatou, Fernando Ania and Araceli Flores
The Journal of Physical Chemistry C
DOI: 10.1021/jp309067e
Link to full article