Atomic Layer Deposition of Platinum Nanocatalysts onto Three-Dimensional Carbon Nanotube/Graphene Hybrid

Chien-Te Hsieh, Yung-Ying Liu, Dong-Ying Tzou and Wei-Yu Chen



TOC Graphic


The Journal of Physical Chemistry C

DOI: 10.1021/jp303552j






Link to full article