Sub-nanometer Atomic Layer Deposition for Spintronics in Magnetic Tunnel Junctions Based on Graphene Spin-Filtering Membranes

TOC Graphic


ACS Nano

DOI: 10.1021/nn5017549




Marie-Blandine Martin, Bruno Dlubak, Robert S. Weatherup, Heejun Yang, Cyrile Deranlot, Karim Bouzehouane, Frédéric Petroff, Abdelmadjid Anane, Stephan Hofmann, John Robertson, Albert Fert and Pierre Seneor