Atomic Layer Deposition of FeO on Pt(111) by Ferrocene Adsorption and Oxidation
Chemistry of Materials
DOI: 10.1021/acs.chemmater.5b01778
Rajib Paul, Ronald G. Reifenberger, Timothy S. Fisher and Dmitry Y. Zemlyanov