Nanoindentation cannot accurately predict the tensile strength of graphene or other 2D materials

Nanoscale, 2015, Accepted Manuscript
DOI: 10.1039/C5NR04134A, Paper
Jihoon Han, Nicola Pugno, Seunghwa Ryu
Due to the difficulty of performing uniaxial tensile testing, the strengths of graphene and its grain boundaries have been measured in experiments by nanoindentation testing. From a series of molecular...