Tuesday, November 12, 2013

Atomic Layer Deposition of BiFeO3 Thin Films Using β-Diketonates and H2O

TOC Graphic


The Journal of Physical Chemistry C

DOI: 10.1021/jp4080652




Feng Zhang, Guosheng Sun, Wanshun Zhao, Lei Wang, Liu Zheng, Shengbei Liu, Bin Liu, Lin Dong, Xingfang Liu, Guoguo Yan, Lixin Tian and Yiping Zeng

Click for full article