Atomic Layer Deposition of Gallium Sulfide Films Using Hexakis(dimethylamido)digallium and Hydrogen Sulfide
Chemistry of Materials
DOI: 10.1021/cm4031057
Xiangbo Meng, Joseph A. Libera, Timothy T. Fister, Hua Zhou, Jenny K. Hedlund, Paul Fenter and Jeffrey W. Elam