Anisotropic Atomic Layer Deposition Profiles of TiO2 in Hierarchical Silica Material with Multiple Porosity

Sreeprasanth Pulinthanathu Sree, Jolien Dendooven, Jasper Jammaer, Kasper Masschaele, Davy Deduytsche, Jan D'Haen, Christine E. A. Kirschhock, Johan A. Martens and Christophe Detavernier