Atomic Layer Deposition of Platinum Nanocatalysts onto Three-Dimensional Carbon Nanotube/Graphene Hybrid
Chien-Te Hsieh, Yung-Ying Liu, Dong-Ying Tzou and Wei-Yu Chen
The Journal of Physical Chemistry C
DOI: 10.1021/jp303552j
Link to full article