Nanoscale , 2013, Advance Article
DOI: 10.1039/C3NR02086J, Paper
DOI: 10.1039/C3NR02086J, Paper
Guoyong Fang, Jing Ma
DFT calculations revealed that the rapid atomic layer deposition of silica nanolaminate is synergistically catalyzed by the formation of the [AlOx ] site and interfacial hydrogen bonding interactions.
To cite this article before page numbers are assigned, use the DOI form of citation above.
The content of this RSS Feed (c) The Royal Society of Chemistry
DFT calculations revealed that the rapid atomic layer deposition of silica nanolaminate is synergistically catalyzed by the formation of the [AlOx ] site and interfacial hydrogen bonding interactions.